Wire rope electric hoist after using a period of time, the gears will wear.
Transmission gear for electric wire rope hoist on another failure form is abrasion,tooth wear after thinning. If the lubrication wear caused by impurities, commonly known as the abrasive wear. This wear often appear in the addendum and dedendumscraping together the very deep, scraping the road perpendicular to the pitch line and parallel to each other. After scraping the oil temperature crane series
rise, reducer, geartransmission shrill noise, then must replace the lubricating oil.lift hoist
The tooth form deviation, deviation installation center distance is too large, can cause the top edge and the root part of the transition curve excessive squeeze gears, thetooth fillet part produces severe wear. Due to overload, often make tooth driving wheel or gear tooth top (and sometimes along the whole tooth surface) is worn verythin layer.
electric chain hoist and trolley mechanism speed reducer gear wear, tooth thickness should not be less than the original tooth thickness of 60%, for running gear wear tooth thickness should not be less than the original tooth thickness of 80%, more than the standard should be replaced with new gear. Thickness of tooth wear can be used to measure toothcaliper measurement of tooth thickness test. The measurement method is shown in figure. Gear measuring caliper is comprehensive caliper vernier caliper and a depth gauge, used to measure thickness of tooth. When measuring, first from the drawingsfound tooth height (i.e. from the pitch circle and addendum height), the tooth thickness caliper vertical scale to this height. Then, the card foot got stuck teeth, with horizontal scale measurement of tooth thickness. The measurement precision can reach 0.02mm.
没有评论:
发表评论